Recommended Process Flow
1. Foundation Treatment
• Inspect the foundation: Ensure that the concrete or asphalt foundation is flat, solid, clean, without cracks or chipping.
• Clean the surface: Sweep away dust and debris. If necessary, use high-pressure water to rinse.
• Leveling Treatment: Use cement mortar or repair materials to fill in the potholes to ensure a flat surface.
2. Base Layer Installation (Buffer Layer)
• Materials: Black PU glue + SBR particles (common particle size 1-3mm).
• Construction Steps:
1. Mix SBR particles with the special glue in the prescribed ratio (common ratios 1:7 or 1:8).
2. Spread the mixture evenly to the specified thickness (usually 8-10mm).
3. Use a roller to flatten and compact, ensuring a uniform surface.
4. Curing Time: Approximately 24 hours (adjust according to temperature and humidity).
3. Top Layer Installation (EPDM Layer)
• Materials: Colored EPDM particles + PU glue.
• Construction Steps:
1. Mix EPDM particles with the glue in the prescribed ratio (usually 1:6 or 1:7).
2. Spread it evenly on the buffer layer, with a thickness of 3-4mm (up to 5-8mm for kindergartens).
3. Use a trowel or scraper to compact and smooth the surface, ensuring the particles are dense and not loose.
4. Curing Time: Approximately 24 hours.
4. Surface Finishing
• Clean up excess materials at the edges and joints.
• Spray surface protection agent as needed to enhance wear resistance and waterproofing.
• After complete curing, check for any particle detachment or hollow areas and repair them.
What Is The Recommended Process For Laying EPDM Granules? What Supporting Materials Are Required?